Polymer Property : Cure Time = 13.5 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 5.50 - 13.5 min
0.0917 - 0.225 hour
t`90; ASTM D2084
ExxonMobil Exxon™ 2211 Fast Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber balesInformation provided by ExxonMobil Chemical