Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 60.0 - 90.0 min | 1.00 - 1.50 hour | handling time |
Permabond ET536 Epoxy Resin PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo.. |
|||
Cure Time | 60.0 - 90.0 min @Temperature 149 - 177 °C |
1.00 - 1.50 hour @Temperature 300 - 350 °F |
|
Master Bond EP13 High Temperature Resistant One Component Epoxy System Master Bond Polymer System EP13 is a one component heat curing epoxy featuring high shear strength and very high temperature resistance. EP13 forms rigid and dimensionally stable bonds with minimal .. |
|||
Cure Time | 60.0 - 90.0 min @Temperature 149 - 177 °C |
1.00 - 1.50 hour @Temperature 300 - 350 °F |
|
Master Bond EP15 High Tensile Strength One Component Epoxy Master Bond Polymer System EP15 is a one component, heat curing epoxy featuring high tensile strength utilized in testing the adhesion and/or cohesive strength of flame-sprayed coatings. This standa.. |
|||
Cure Time | 45.0 - 90.0 min @Temperature 22.0 °C |
0.750 - 1.50 hour @Temperature 71.6 °F |
|
Dow Corning 3-4150 DIELECTRIC GEL KIT Two-part, transparent green, fast RT or heat cure.Information provided by Dow Corning |
|||
Cure Time | 30.0 - 90.0 min @Temperature 100 - 160 °C |
0.500 - 1.50 hour @Temperature 212 - 320 °F |
or longer |
Abatron AboCoat 8204-15/AboCure 8204-15 Epoxy Coating AboCoat 8204-15 is a flammable light-blue liquid resin. AboCure 8204-115 is a flammable clear amber liquid converter. AboCoat 8204-15/AboCure 8204-15 is a dielectric coating for high chemical, solve.. |
|||
Cure Time | 60.0 - 90.0 min | 1.00 - 1.50 hour | Hard Dry |
3M Scotchkote™ XF 895 Fast Curing Floor Coating Scotchkote Fast Curing Floor Coating XF 895 has been specifically developed as a high build floor protection system for application to concrete surfaces, to provide rapid return to serviceProduct Fe.. |
|||
Cure Time | 60.0 - 90.0 min | 1.00 - 1.50 hour | Tack-Free, 50% RH |
3M 540 Polyurethane Sealant 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
Cure Time | 50.0 - 90.0 min | 0.833 - 1.50 hour | Tack-Free, 50% RH |
3M 550 Polyurethane Adhesive Sealant Fast Cure 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |