Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | On Steel (Fixture) |
ND Industries 306 Surface Insensitive Instant Superglue Low viscosity for difficult to bond rubber compounds |
|||
Cure Time | 0.500 - 0.583 min | 0.00833 - 0.00972 hour | Aluminum, handling time |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Cure Time | 0.500 - 0.583 min | 0.00833 - 0.00972 hour | Aluminum, set time, cured |
Permabond 738 Cyanoacrylate, toughened PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over.. |
|||
Cure Time | 0.417 - 0.583 min | 0.00694 - 0.00972 hour | Metal set time |
Lord Adhesives 5019 Fast Setting, High Elasticity, High Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.500 - 0.583 min | 0.00833 - 0.00972 hour | Plastic set time |
Lord Adhesives 5181 High Viscosity, Black, General Purpose Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.500 - 0.583 min | 0.00833 - 0.00972 hour | Rubber set time |
Lord Adhesives 5181 High Viscosity, Black, General Purpose Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.417 - 0.583 min | 0.00694 - 0.00972 hour | Metal set time |
Lord Adhesives 7700 Fast Setting, High Viscosity, Impact Resistant. Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.267 - 0.583 min | 0.00444 - 0.00972 hour | Tack Free Time |
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim.. |
|||
Cure Time | 0.267 - 0.583 min | 0.00444 - 0.00972 hour | Tack Free Time |
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr.. |
|||
Cure Time | 0.267 - 0.583 min | 0.00444 - 0.00972 hour | Tack Free Time |
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa.. |
|||
Cure Time | 0.267 - 0.583 min | 0.00444 - 0.00972 hour | Tack Free Time |
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL.. |
|||
Cure Time | 0.267 - 0.583 min | 0.00444 - 0.00972 hour | Tack Free Time |
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi.. |
|||
Cure Time | 0.167 - 0.583 min | 0.00278 - 0.00972 hour | Time to Handling Strength |
3M Scotch-Weld™ FLX300 Flexible Instant Adhesive 3M™ Scotch-Weld™ Flexible Instant Adhesive FLX (formerly PR851) is formulated for extended resistance to impact, vibration, stress, peel, and humidity applications. It is faster curing than 3M™ S.. |
|||
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | Time to Handling Strength |
3M Scotch-Weld™ MC5 Metal Instant Adhesive 3M™ Scotch-Weld™ Metal Instant Adhesives are designed to give optimum performance and high strength bonds on metals, including galvanized or anodized surfaces. MC5 (formerly SP93) is a very low vi.. |
|||
Cure Time | 0.333 - 0.583 min | 0.00555 - 0.00972 hour | Time to Handling |
3M Scotch-Weld™ MG300 FLX Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.267 - 0.583 min | 0.00444 - 0.00972 hour | Tack Free Time |
ACC EP RP EPI Engineered Polymers Aromatic Polyurea EP RP, Aromatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RP displays extremely fast cure time.. |
|||
Cure Time | 0.267 - 0.583 min | 0.00444 - 0.00972 hour | Tack Free Time |
ACC EP RSP EPI Engineered Polymers Silicone Polyurea EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time.. |
|||
Cure Time | 0.267 - 0.583 min | 0.00444 - 0.00972 hour | Tack Free Time |
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti.. |
|||
Cure Time | 0.417 - 0.583 min | 0.00694 - 0.00972 hour | per mm |
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation
Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche.. |
|||
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | Time to Handling Strength |
3M Scotch-Weld™ SI5 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI5 (formerly SB20) is a very l.. |
|||
Cure Time | 0.267 - 0.583 min | 0.00444 - 0.00972 hour | Tack Free Time |
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst.. |