Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries 301 Surface Insensitive Instant Superglue Low-medium viscosity for difficult to bond substrates |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries 331 Surface Insensitive Instant Superglue Medium-high viscosity for difficult to bond surfaces |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries 333 Surface Insensitive Instant Superglue Low-medium viscosity for difficult to bond substrates |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | on metal (Fixture) |
ND Industries 621 Heptane-Acetone SuperGlue accelerator Fast acting SuperGlue accelerator 15 seconds. Non-ozone depleting but flammable solvent |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 314 General DescriptionA medium viscosity ethyl-based cyanoacrylate particularly suitable for rubbers and plastics. It is fast acting and may be fillet cured using ND Excel Accelerators.rubber O-rings,.. |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 325 Low-Medium Viscosity - General purposeMeets military spec Mil-A-46050C Type II Class I |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Buna N Rubber, handling time |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Neoprene, handling time |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Steel, handling time |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Cure Time | <= 0.250 min | <= 0.00417 hour | NBR Rubber, handling time |
Permabond 922 Cyanoacrylate, High temperature PERMABOND® 922 is the original allyl cyanoacrylate adhesive. It is a single part, moderate viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. P.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6011 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6012 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | <= 0.250 min | <= 0.00417 hour | zinc, fixture time with initiator 44 |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Cure Time | 0.250 - 0.500 min | 0.00417 - 0.00833 hour | zinc, fixture time with initiator 43 |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6403 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6602 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6813 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.250 min | 0.00417 hour | Steel, set time |
Permabond 200 Cyanoacrylate, wire tacking PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Cure Time | 0.250 min | 0.00417 hour | Buna N Rubber, set time |
Permabond 200 Cyanoacrylate, wire tacking PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Steel, handling time |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Buna N Rubber, handling time |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Phenolic, handling time |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Steel, handling time |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6812 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.250 min | 0.00417 hour | |
Loctite® 406 Surface Insensitive Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Cure Time | 0.250 min | 0.00417 hour | |
Loctite® 412 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | Time to Handling Strength |
3M Scotch-Weld™ HT700 High Temperature Instant Adhesive 3M™ Scotch-Weld™ High Temperature Instant Adhesives provide superior performance for demanding applications where high temperatures, thermal cycling, or shock resistance is required. HT700 is a me.. |
|||
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | Time to Handling Strength |
3M Scotch-Weld™ MC5 Metal Instant Adhesive 3M™ Scotch-Weld™ Metal Instant Adhesives are designed to give optimum performance and high strength bonds on metals, including galvanized or anodized surfaces. MC5 (formerly SP93) is a very low vi.. |
|||
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | Time to Handling Strength |
3M Scotch-Weld™ SI5 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI5 (formerly SB20) is a very l.. |
|||
Cure Time | 0.250 - 0.417 min | 0.00417 - 0.00694 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |