Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 5.50 - 13.5 min | 0.0917 - 0.225 hour | t`90; ASTM D2084 |
ExxonMobil Exxon™ 2211 Fast Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber balesInformation provided by ExxonMobil Chemical |