Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | >= 0.125 min | >= 0.00208 hour | Fixture |
Resinlab® CYNERGY CA6305 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Cure Time | >= 0.125 min | >= 0.00208 hour | Fixture |
Resinlab® CYNERGY CA6308 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Cure Time | >= 0.125 min | >= 0.00208 hour | Fixture |
Resinlab® CYNERGY CA6309 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Cure Time | >= 0.125 min | >= 0.00208 hour | Fixture |
Resinlab® CYNERGY CA6306 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Cure Time | >= 0.125 min | >= 0.00208 hour | Fixture |
Resinlab® CYNERGY CA6307 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |