Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries 301 Surface Insensitive Instant Superglue Low-medium viscosity for difficult to bond substrates |
|||
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | On Steel (Fixture) |
ND Industries 306 Surface Insensitive Instant Superglue Low viscosity for difficult to bond rubber compounds |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries 360 Surface Insensitive Instant Superglue General DescriptionA medium viscosity, general purpose cyanoacrylate which is also surface sensitive. Can handle a wide array of materials which include wood, cork, leather, stone and plastics, in .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | on metal (Fixture) |
ND Industries 621 Heptane-Acetone SuperGlue accelerator Fast acting SuperGlue accelerator 15 seconds. Non-ozone depleting but flammable solvent |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 314 General DescriptionA medium viscosity ethyl-based cyanoacrylate particularly suitable for rubbers and plastics. It is fast acting and may be fillet cured using ND Excel Accelerators.rubber O-rings,.. |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 325 Low-Medium Viscosity - General purposeMeets military spec Mil-A-46050C Type II Class I |
|||
Cure Time | 0.250 min | 0.00417 hour | Buna N Rubber, handling time |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Buna N Rubber, handling time |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Steel, handling time |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Cure Time | <= 0.250 min | <= 0.00417 hour | NBR Rubber, handling time |
Permabond 922 Cyanoacrylate, High temperature PERMABOND® 922 is the original allyl cyanoacrylate adhesive. It is a single part, moderate viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. P.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6009 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6014 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 0.250 - 0.500 min | 0.00417 - 0.00833 hour | zinc, fixture time with initiator 43 |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Cure Time | 0.250 - 0.500 min | 0.00417 - 0.00833 hour | zinc, fixture time with initiator 44 |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6403 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6702 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6813 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Steel, handling time |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Cure Time | <= 0.250 min | <= 0.00417 hour | NBR Rubber, handling time |
Permabond 919 Cyanoacrylate, High temperature Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6402 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6810 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6811 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.250 - 0.417 min | 0.00417 - 0.00694 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
Cure Time | 0.250 - 0.417 min | 0.00417 - 0.00694 hour | Metal set time |
Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.250 min | 0.00417 hour | |
Loctite® PRISM® 454 Instant Adhesive Gel Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Cure Time | 0.250 min | 0.00417 hour | Set Time |
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | Time to Handling Strength |
3M Scotch-Weld™ HT700 High Temperature Instant Adhesive 3M™ Scotch-Weld™ High Temperature Instant Adhesives provide superior performance for demanding applications where high temperatures, thermal cycling, or shock resistance is required. HT700 is a me.. |
|||
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | Time to Handling Strength |
3M Scotch-Weld™ MC5 Metal Instant Adhesive 3M™ Scotch-Weld™ Metal Instant Adhesives are designed to give optimum performance and high strength bonds on metals, including galvanized or anodized surfaces. MC5 (formerly SP93) is a very low vi.. |
|||
Cure Time | 0.250 - 10100 min | 0.00417 - 168 hour | Average value: 489 min Grade Count:28 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Cure Time | 0.250 min | 0.00417 hour | |
Loctite® PRISM® 401 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |