Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | >= 0.200 min | >= 0.00333 hour | Fixture |
Resinlab® CYNERGY CA6008 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.200 min | >= 0.00333 hour | Fixture |
Resinlab® CYNERGY CA6502 Adhesive Description: The CYNERGY 6500 SERIES are black, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Cure Time | >= 0.200 min | >= 0.00333 hour | Fixture |
Resinlab® CYNERGY CA6902 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Cure Time | >= 0.200 min | >= 0.00333 hour | Fixture |
Resinlab® CYNERGY CA6808 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.200 - 0.250 min | 0.00333 - 0.00417 hour | Rubber set time |
Lord Adhesives CA High Viscosity, General Purpose, Non Stringing, Non Migrating Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.200 - 0.333 min | 0.00333 - 0.00556 hour | per mm |
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Cure Time | 0.200 - 0.333 min | 0.00333 - 0.00556 hour | per mm |
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Cure Time | 0.200 - 0.333 min | 0.00333 - 0.00556 hour | per mm |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |