Polymer Property : Cure Time = 0.00283 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 0.170 min
0.00283 hour
Fixture time @ 70 - 100 mW/cm^2
Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
Cure Time 0.170 min
0.00283 hour
Fixture time @ 150 mW/cm^2
Loctite® 3872 1 component acrylic/urethane UV/Heat Cure Flexible Adhesive
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
Cure Time 0.170 min
0.00283 hour
Loctite® 4471 Surface Insensitive Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..