Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | >= 0.133 min | >= 0.00222 hour | Fixture |
Resinlab® CYNERGY CA6205 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | >= 0.133 min | >= 0.00222 hour | Fixture |
Resinlab® CYNERGY CA6206 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | 0.133 min | 0.00222 hour | Steel, handling time |
Permabond 799 Cyanoacrylate, Surface insensitive PERMABOND® 799 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Cure Time | 0.133 min | 0.00222 hour | Buna N Rubber, handling time |
Permabond 799 Cyanoacrylate, Surface insensitive PERMABOND® 799 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Cure Time | 0.133 min | 0.00222 hour | Phenolic, handling time |
Permabond 799 Cyanoacrylate, Surface insensitive PERMABOND® 799 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Cure Time | >= 0.133 min | >= 0.00222 hour | Fixture |
Resinlab® CYNERGY CA6004 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.133 min | >= 0.00222 hour | Fixture |
Resinlab® CYNERGY CA6102 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Cure Time | >= 0.133 min | >= 0.00222 hour | Fixture |
Resinlab® CYNERGY CA6203 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | >= 0.133 min | >= 0.00222 hour | Fixture |
Resinlab® CYNERGY CA6204 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | >= 0.133 min | >= 0.00222 hour | Fixture |
Resinlab® CYNERGY CA6207 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | >= 0.133 min | >= 0.00222 hour | Fixture |
Resinlab® CYNERGY CA6804 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.133 min | 0.00222 hour | Hot tack |
Valley Adhesives EM-490 High Temperature Application Glue Stick Valley Adhesives EM-490 High Temperature Application Glue StickExcellent tack; Used on plastics, metals and other surfaces. |
|||
Cure Time | 0.133 min | 0.00222 hour | Hot tack |
Valley Adhesives EM-500 High Temperature Application Glue Stick Valley Adhesives EM-500 High Temperature Application Glue StickHi and low temperature general purpose; Bonds P.O.P. displays, porous and non-porous substrates, paper, corrugated boxes, fabrics, and .. |
|||
Cure Time | 0.133 min | 0.00222 hour | Hot tack |
Valley Adhesives EM-900 High Temperature Application Glue Stick Valley Adhesives EM-900 High Temperature Application Glue StickGeneral purpose; Bonds P.O.P. displays, porous and non-porous substrates, paper, corrugated boxes, fabrics, and foams. |