Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.100 min | 0.00167 hour | Steel, set time |
Permabond 798 Cyanoacrylate, Surface insensitive PERMABOND 798 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, Metals, Ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Cure Time | 0.100 min | 0.00167 hour | Buna N Rubber, set time |
Permabond 798 Cyanoacrylate, Surface insensitive PERMABOND 798 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, Metals, Ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Cure Time | 0.100 min | 0.00167 hour | Phenolic, set time |
Permabond 798 Cyanoacrylate, Surface insensitive PERMABOND 798 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, Metals, Ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Cure Time | 0.100 min | 0.00167 hour | fixture time, (low power 4mW lamp) |
Permabond UV630 UV-curable Adhesive PERMABOND UV630 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Cure Time | 0.100 - 0.167 min | 0.00167 - 0.00278 hour | Plastic set time |
Lord Adhesives 5019 Fast Setting, High Elasticity, High Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.100 - 0.133 min | 0.00167 - 0.00222 hour | Plastic set time |
Lord Adhesives 6900 Medium Viscosity, Low Odor, Low Bloom Butyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |