Processing Properties Metric English Comments
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
PolyOne Versalloy™ HC 9210-45N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-45N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgic..
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod..
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
PolyOne Versalloy™ XL 9045-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9045-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp..
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE)
Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p..
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1000 thermoplastic polyolefin elastomer has been developed for applications that require impact resistance and a high gloss scratch and mar resistant surface finish. Elastocon® SMR10..
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
Elastocon TPE Technologies Elastocon® SMR1450 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1450 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1555 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
Elastocon TPE Technologies Elastocon® SMR1600 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1600 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..