Polymer Property : Back Pressure = 50.8 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 0.150 - 0.350 MPa
21.8 - 50.8 psi
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF
A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Back Pressure 0.000 - 0.350 MPa
0.000 - 50.8 psi
BASF Ultramid® N-276 BK ND 3007 40% Glass/Mineral Filled PA66
Description: Ultramid N-276 BK ND3007 is a 40% mineral/glass reinforced, heat stabilized injection molding PA6/6.Information provided by BASF
Back Pressure 0.000 - 0.350 MPa
0.000 - 50.8 psi
BASF Ultramid® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Conditioned)
Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio..
Back Pressure 0.000 - 0.350 MPa
0.000 - 50.8 psi
BASF Ultramid® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Dry)
Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio..
Back Pressure 0.000 - 0.350 MPa
0.000 - 50.8 psi
BASF Ultramid® AZ HP UV BK 23220 PA66 (Dry)
Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 o..
Back Pressure 0.150 - 0.350 MPa
21.8 - 50.8 psi
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF
A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Back Pressure 0.150 - 0.350 MPa
21.8 - 50.8 psi
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF
A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Back Pressure 0.150 - 0.350 MPa
21.8 - 50.8 psi
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber
A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.