Processing Properties Metric English Comments
Back Pressure 0.000 - 4.02 MPa
0.000 - 583 psi
Injection Molding
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity
Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
Back Pressure 0.000 - 4.02 MPa
0.000 - 583 psi
Injection Molding
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity
Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
Back Pressure 0.000 - 4.02 MPa
0.000 - 583 psi
Injection Molding
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity
Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical