Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 4.02 - 8.04 MPa | 583 - 1170 psi | Injection Molding |
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Back Pressure | 4.02 - 8.04 MPa | 583 - 1170 psi | Injection Molding |
LG Chemical LUCEL N109LDS POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Back Pressure | 4.02 - 8.04 MPa | 583 - 1170 psi | Injection Molding |
LG Chemical LUCEL N109WR POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Back Pressure | 4.02 - 8.04 MPa | 583 - 1170 psi | Injection Molding |
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Back Pressure | 4.02 - 8.04 MPa | 583 - 1170 psi | Injection Molding |
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |