Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 241-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Vyram™ 9103-54 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Vyram™ 9203-45 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Vyram™ 9203-54 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 121-67W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 241-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 241-73W236 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and contains.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 203-50 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Back Pressure | 10.0 - 20.0 MPa | 1450 - 2900 psi | |
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 241-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Vyram™ 9201-45 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |