Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-113 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-1162 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-117 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-220 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-301 Flame Retardant Polystyrene Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-702 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-960 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingPrinter and photocopier .. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-960PC Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmNon-DPO, UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housingInforma.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-980 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOExcellent heat stability & electrical propertyColor tailor-made for clientApplications:Injection moldingGas assistant mold.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa HIPS-5197 High Impact Polystyrene Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-100 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mmLow smoking, low halogenExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV or aud.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-8002 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPS-930 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, 5VA @ 2.6mmNon-DPO, high UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingPrinter, photocopier, fax machineElec.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Kingfa FRHIPSV-0 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingTV or aud.. |
|||
Back Pressure | 0.500 - 15.0 MPa | 72.5 - 2180 psi | Injection Molding |
LG Chemical LUTENE-H ME6000 HDPE Description: LUTENE-H ME6000 is mainly intended for injection molding of crates. It has excellent mechanical properties and high impact strength.Applications: Transport and stacking crates, bottle c.. |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Zhejiang Juner 301-G0 Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Beijing Chemical Industry KAIFA® 301-G10 PBT Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Beijing Ranger Chem PBT 403 M-G0 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Beijing Ranger Chem PBT 403 M-G10 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Beijing Ranger Chem PBT-201-G0 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Beijing Ranger Chem PBT-201-G0 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Beijing Ranger Chem PBT-201-G10 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Beijing Ranger Chem PBT-201-G0 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Beijing Chemical Industry KAIFA® 301-G0 PBT Resin Flame retardant, folding enduranceInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Back Pressure | 0.500 - 15.0 MPa | 72.5 - 2180 psi | Injection Molding |
LG Chemical LUTENE-H ME8000 HDPE Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.Applications: Silicone cartridge, containers, complicated.. |
|||
Back Pressure | 4.00 - 15.0 MPa | 580 - 2180 psi | |
Beijing Ranger Chem PBT 403 M-G0 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |