Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.150 - 0.350 MPa | 21.8 - 50.8 psi | |
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Back Pressure | 0.000 - 0.350 MPa | 0.000 - 50.8 psi | |
BASF Ultramid® N-276 BK ND 3007 40% Glass/Mineral Filled PA66 Description: Ultramid N-276 BK ND3007 is a 40% mineral/glass reinforced, heat stabilized injection molding PA6/6.Information provided by BASF |
|||
Back Pressure | 0.000 - 0.350 MPa | 0.000 - 50.8 psi | |
BASF Ultramid® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Conditioned) Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio.. |
|||
Back Pressure | 0.000 - 0.350 MPa | 0.000 - 50.8 psi | |
BASF Ultramid® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Dry) Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio.. |
|||
Back Pressure | 0.000 - 0.350 MPa | 0.000 - 50.8 psi | |
BASF Ultramid® AZ HP UV BK 23220 PA66 (Dry) Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 o.. |
|||
Back Pressure | 0.150 - 0.350 MPa | 21.8 - 50.8 psi | |
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Back Pressure | 0.150 - 0.350 MPa | 21.8 - 50.8 psi | |
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Back Pressure | 0.150 - 0.350 MPa | 21.8 - 50.8 psi | |
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |