Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2 - 8 hour | 2 - 8 hour | in desiccant air dryer |
Polykemi AB POLYblend 45FS GKF2505 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in fresh-air dryer |
Polykemi AB POLYblend 45H PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in desiccant air dryer |
Polykemi AB POLYblend 45H PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in desiccant air dryer |
Polykemi AB POLYblend 45V PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in circulation dryer |
Polykemi AB POLYblend 50LG PC/ABS-Blend, Low Gloss Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in desiccant air dryer |
Polykemi AB POLYblend 65H PC/ABS-Blend Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in fresh-air dryer |
Polykemi AB POLYblend 65V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in desiccant air dryer |
Polykemi AB POLYblend 65V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in circulation dryer |
Polykemi AB POLYblend 85V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in circulation dryer |
Polykemi AB POLYblend C65HF PC/ABS-blend Information provided by Polykemi AB |
|||
Dry Time | 4 - 8 hour | 4 - 8 hour | |
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030JI9L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability, designed for high burst pressure performance at high temperat.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Nitric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 4 - 8 hour | 4 - 8 hour | |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Dry Time | 4 - 8 hour | 4 - 8 hour | |
Beijing Chemical Industry KAIFA® 2030 PET Resin High mechanical strength, Creep resistant, Low frictionInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | |
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer
(discontinued **) XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder tempe.. |