Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 70.0 - 88.0 °C | 158 - 190 °F | Average value: 77.4 °C Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Drying Temperature | 85.0 - 88.0 °C | 185 - 190 °F | Average value: 87.3 °C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |