Processing Properties Metric English Comments
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant
Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant
Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Drying Temperature 143 - 149 °C
290 - 300 °F
Average value: 148 °C Grade Count:3
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-GP1 Polyetherimide, General Purpose, Unreinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 143 - 149 °C
290 - 300 °F
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.