Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP) Information provided by PolyOne |
|||
Drying Temperature | <= 135 °C | <= 275 °F | |
Oxford Polymers PEI 1000 PEI Product Description: (Unreinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Colors AvailableInformation provided.. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Drying Temperature | <= 135 °C | <= 275 °F | |
Oxford Polymers PEI 1010 PEI Product Description: (Unreinforced), Polyetherimide injection molding grade, high flow Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: .. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | Average value: 147 °C Grade Count:8 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 135 °C | 275 °F | |
PolyOne Stat-Tech™ PI-05CF/000 Polyetherimide - 5% Carbon Fibers - ESD Applications
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding Information provided by PolyOne™ Corporation |
|||
Drying Temperature | 135 - 163 °C | 275 - 325 °F | |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
Drying Temperature | 135 - 163 °C @Time 10800 - 14400 sec |
275 - 325 °F @Time 3.00 - 4.00 hour |
|
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
Drying Temperature | 135 - 149 °C | 275 - 300 °F | |
PolyOne Lubri-Tech™ SF-25GF/13T BLACK Polyphenylene Sulfide (PPS), Glass Filled, PTFE Lubricated
(discontinue Description/Features:Glass Fiber ReinforcedPTFE LubricatedBlackPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 135 - 163 °C @Time 12600 sec |
275 - 325 °F @Time 3.50 hour |
|
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU) Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro.. |
|||
Drying Temperature | 135 °C | 275 °F | |
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications
&a Data provided by PolyOne. |
|||
Drying Temperature | 135 °C | 275 °F | |
PolyOne Edgetek® SF-10GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |