Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1200-7116 ABS, with carbon fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1200-8493 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 65-7311 PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 65-7712/GY PP-copolymer, with carbon fiber and glass fiber, electrically conducting Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG.. |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b.. |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 65-8347/RD PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 65-8452-1 PP-copolymer, with aramid reinforcement, lubricant modified Applications: Office communication.Low warpage, isotropic shrinkage characteristics.Dynamic stressed parts.Information provided by Lehmann & Voss & Co.KG |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 65-8452-2 PP-copolymer, with carbon fiber, aramid reinforcement, lubricant modified Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Information provided by.. |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 65-8498 PP-copolymer, unreinforced Applications: Office communication.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable for thin wall complex parts.Information provided by Lehmann & Voss &.. |
|||
Drying Temperature | 85.0 - 95.0 °C | 185 - 203 °F | Injection Molding |
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p.. |
|||
Drying Temperature | 85.0 - 95.0 °C | 185 - 203 °F | Injection Molding |
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Drying Temperature | 85.0 - 95.0 °C | 185 - 203 °F | Injection Molding |
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an.. |
|||
Drying Temperature | 85.0 - 95.0 °C | 185 - 203 °F | Injection Molding |
LG Chemical LUPOY GP5100 PC/ABS+GF10% Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by.. |
|||
Drying Temperature | 85.0 - 95.0 °C @Time 7200 - 18000 sec |
185 - 203 °F @Time 2.00 - 5.00 hour |
|
IRPC Polimaxx Porene KU200 Acrylonitrile Butadiene Styrene Applications:extrusion applicationautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances |
|||
Drying Temperature | 85.0 - 95.0 °C @Time 7200 - 18000 sec |
185 - 203 °F @Time 2.00 - 5.00 hour |
|
IRPC Polimaxx Porene KU650 Acrylonitrile Butadiene Styrene Applications:injection moldingautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Drying Temperature | 85.0 - 95.0 °C | 185 - 203 °F | |
Kostat BK-STAT 7048BK ABS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Drying Temperature | 85.0 - 95.0 °C | 185 - 203 °F | |
Kostat BK-STAT 7048BK ABS Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |
|||
Drying Temperature | 80.0 - 95.0 °C | 176 - 203 °F | |
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 70.0 - 95.0 °C | 158 - 203 °F | Average value: 81.2 °C Grade Count:20 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Drying Temperature | 70.0 - 95.0 °C @Time 7200 - 14400 sec |
158 - 203 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1200-7116-2 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |
|||
Drying Temperature | 85.0 - 95.0 °C | 185 - 203 °F | Pre-drying |
Styrolution Luran® S KR 2867 C WU Colored ASA+PC Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO.. |