Processing Properties Metric English Comments
Drying Temperature 170 °C
338 °F
> 4 hours hopper drying with desiccated air inlet for extrusion
Solvay Specialty Polymers Supradel® HTS-2630 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2630 is a 30% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..
Drying Temperature 170 °C
338 °F
> 4 hours hopper drying with desiccated air inlet for extrusion
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin  (discontinued **)
Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o..
Drying Temperature 170 °C
338 °F
> 4 hours hopper drying with desiccated air inlet for extrusion
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2..
Drying Temperature 170 °C
338 °F
> 4 hours hopper drying with desiccated air inlet for extrusion
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of ..
Drying Temperature 170 °C
338 °F
> 4 hours hopper drying with desiccated air inlet for extrusion
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t..
Drying Temperature 170 °C
338 °F
> 4 hours hopper drying with desiccated air inlet for extrusion
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin  (discontinued **)
Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i..
Drying Temperature 170 °C
338 °F
> 4 hours hopper drying with desiccated air inlet for extrusion
Solvay Specialty Polymers Supradel® HTS-2620 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2620 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..
Drying Temperature 170 °C
338 °F
> 4 hours hopper drying with desiccated air inlet for extrusion
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the..