Processing Properties Metric English Comments
Drying Temperature 116 - 135 °C
240 - 275 °F
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled  (discontinued **)
Information provided by MRC Polymers Inc.
Drying Temperature 79.4 - 135 °C
175 - 275 °F
Average value: 103 °C Grade Count:16
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Drying Temperature 121 - 135 °C
250 - 275 °F
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated  (discontinued **)
Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Drying Temperature 121 - 135 °C
250 - 275 °F
PolyOne Stat-Tech™ PF-05CF/000 EM FR Flame Retardant Polysulfone - 5% Carbon Fiber  (discontinued **)
Data provided by PolyOne.
Drying Temperature 120 - 135 °C

@Time 14400 sec
248 - 275 °F

@Time 4.00 hour
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
Drying Temperature 120 - 135 °C

@Time 14400 sec
248 - 275 °F

@Time 4.00 hour
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
Drying Temperature 120 - 135 °C
248 - 275 °F
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl..
Drying Temperature 90.0 - 135 °C
194 - 275 °F
Solvay Specialty Polymers Amodel® A-6625 HS BK324 Polyphthalamide, 25% carbon/glass fiber, ESD grade  (discont
Amodel A-6625 HS BK324 is a 25% carbon and glass-fiber-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This ..
Drying Temperature 121 - 135 °C
250 - 275 °F
Average value: 122 °C Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled