Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-re.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber KetaSpire® KT-820 GF15 is a low flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpir.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 GF20 Polyetheretherketone (PEEK), 20% Glass Fiber KetaSpire® KT-880 GF20 is a high flow, 20% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-351 resin is a higher flow, injection molding grade of PrimoSpire® self-reinforced polyphenylene (SRP). PrimoSpire® SRP resin is an ultra-high performance amorphous, melt-pro.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Rear Barrel Temperature | 365 °C | 689 °F | |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |