Processing Properties Metric English Comments
Rear Barrel Temperature 290 - 300 °C
554 - 572 °F
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement  (discontinu
Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu..
Rear Barrel Temperature 290 - 300 °C
554 - 572 °F
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral  (discontinued **)
Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical..
Rear Barrel Temperature 290 - 300 °C
554 - 572 °F
Solvay Specialty Polymers Primef® 7010 Polyphenylene Sulfide (PPS), 65% GlassMineral  (discontinued **)
Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less flu..
Rear Barrel Temperature 290 - 310 °C
554 - 590 °F
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Rear Barrel Temperature 290 - 310 °C
554 - 590 °F
Unitika PT-3020
Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd.
Rear Barrel Temperature 290 - 310 °C
554 - 590 °F
Unitika P-3001 Engineering Plastic