Polymer Property : Rear Barrel Temperature = 376 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer
A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..