Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 138 - 154 °C | 280 - 310 °F | |
RheTech Products E206-01 Linear Low Density Polyethylene, Black Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |