Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Oxford Polymers Oxnilon 6-60GF(DRY) PA6, 60% Glass Fiber Reinforced, Dry Product Description: Glass Fiber (60% Reinforced), Nylon 6 injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents, Lubricants and Heat Stabiliz.. |
|||
Rear Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Rear Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY6/12-G43 Nylon 612, 43% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources NY66-G20-MD Nylon 66, 20% Glass Reinforced with MoS2 Nylon 66, 20% Glass Reinforced with Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigment.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced Nylon 66, 60% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled PC/ABS Alloy, General Purpose, 20% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources NY66-G55 Nylon 66, 55% Glass Reinforced Nylon 66, 55% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled PC/ABS Alloy, General Purpose, 40% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1212FR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1212FRR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1212FRRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1510FR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1510R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 288 - 288 °C | 550 - 550 °F | |
Star Plastics PC701 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC741 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
Rear Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |