Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 120 °C | 248 °F | For high temperature coextrusions. |
DuPont Bynel® 21E553 Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For film or coating with EVA or EVOH. |
DuPont Bynel® 21E553 Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | |
DuPont Bynel® 30E699 Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | |
DuPont Bynel® 39E622 Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For high temperature coextrusions. |
DuPont Bynel® 41E623 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E623 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For high temperature coextrusions. |
DuPont Bynel® 41E689 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E689 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | |
DuPont Bynel® 30E671 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | |
DuPont Bynel® 3126 Adhesive Resin Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | |
DuPont Bynel® 39E660 Adhesive Resin Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For high temperature coextrusions. |
DuPont Bynel® 4157 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 4157 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For high temperature coextrusions. |
DuPont Bynel® 41E687 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E687 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 42E703 Adhesive Resin Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Rear Barrel Temperature | 120 - 125 °C | 248 - 257 °F | |
BecauseWeCare BF90 Biodegradable Plastic Biodegradable and compostable product produced from corn and developed to break down within weeks in a compost environment, without leaving any harmful residues in the process. Certified to the vari.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For high temperature coextrusions. |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Rear Barrel Temperature | 120 °C | 248 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |