Processing Properties Metric English Comments
Rear Barrel Temperature 213 °C
415 °F
Extrusion
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol
Rear Barrel Temperature 213 °C
415 °F
Lubrizol Estaloc® 59020 Reinforced Thermoplastic Polyurethane
Type: Estaloc® 59020 RETPU is a polyester-type reinforced engineered thermoplastic polyurethane (RETPU).Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact..
Rear Barrel Temperature 213 °C
415 °F
Lubrizol ESTALOC® 60155 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol
Copyright © lookpolymers.com All Rights Reserved