Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 185 - 207 °C | 365 - 405 °F | |
Ineos Nova 50 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High strength crystal polystyrene, High heat crystal polystyrene, Custom colorsApplications: Injection molding or extrusion, Designed for applications requiring strength and high heat resistance whe.. |
|||
Rear Barrel Temperature | 185 - 207 °C | 365 - 405 °F | |
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra.. |