Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 196 - 204 °C | 385 - 399 °F | |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |