Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Rear Barrel Temperature = 191 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 179 - 191 °C
355 - 375 °F
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Rear Barrel Temperature 174 - 191 °C
345 - 375 °F
Elastocon TPE Technologies Elastocon® 8048N Thermoplastic Elastomer
Elastocon® 8048N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8048N is FDA compliant and well suited..
Rear Barrel Temperature 174 - 191 °C
345 - 375 °F
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer
Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui..
Rear Barrel Temperature 174 - 191 °C
345 - 375 °F
Elastocon TPE Technologies Elastocon® 8058HL Thermoplastic Elastomer
Elastocon® 8058HL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058HL is FDA compliant a..
Rear Barrel Temperature 174 - 191 °C
345 - 375 °F
Elastocon TPE Technologies Elastocon® 8058N Thermoplastic Elastomer
Elastocon® 8058N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8058N is FDA compliant and well suited..
Rear Barrel Temperature 177 - 191 °C
350 - 375 °F
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 174 - 191 °C
345 - 375 °F
Elastocon TPE Technologies Elastocon® 8150B Thermoplastic Elastomer
Elastocon® 8150B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8150B is well suited for consumer goods a..
Rear Barrel Temperature 177 - 191 °C
351 - 376 °F
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer
A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Rear Barrel Temperature 177 - 191 °C
350 - 375 °F
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance ..
Copyright © lookpolymers.com All Rights Reserved