Polymer Property : Rear Barrel Temperature = 130 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 130 - 170 °C
266 - 338 °F
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA)
High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Rear Barrel Temperature 130 - 170 °C
266 - 338 °F
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA)
High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Rear Barrel Temperature 130 - 170 °C
266 - 338 °F
Unitika TERRAMAC TE-2000 Polylactic Acid (PLA)
Basic grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.