Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® F7080 Developmental Flame Retardant Polystyrene
(discontinued **) Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj.. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® F7080UV Developmental Flame Retardant Polystyrene
(discontinued **) Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj.. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® F7120 Developmental Flame Retardant Polystyrene
(discontinued **) Features: High flow for thin wall partsGood balance of physical propertiesUL94 V-0 @ 1.5 mm for black color Good aesthetics for injection molding Applications:Large television cabinetsConsumer elect.. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® 7001 High Performance Flame Retardant Polystyrene
(discontinued **) Super high flow, Reduced processing temperatures, Reduced processing time, Improved aesthetics, Custom colorsApplications: Injection molding, Gas-assist injection molding, Hard to fill cavities, suc.. |
|||
Mold Temperature | 32.0 °C | 89.6 °F | |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Mold Temperature | 32.0 °C | 89.6 °F | |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® 7000 Flame Retardant Polystyrene Features:General purpose workhorse resinGood flow for injection moldingUL94 V-0 @ 1.5 mm for all colors UL94 5VA rating FOAMED @ 4.6 mm, 0.87-1.07 g/cc density, natural colorCustom colors availableA.. |
|||
Mold Temperature | 32.0 - 60.0 °C | 89.6 - 140 °F | |
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce.. |
|||
Mold Temperature | 32.0 - 60.0 °C | 89.6 - 140 °F | |
Styrolution NAS® 90 High Performance Styrenic NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla.. |
|||
Mold Temperature | 32.0 - 79.4 °C | 89.6 - 175 °F | Average value: 52.6 °C Grade Count:47 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Mold Temperature | 32.0 °C | 89.6 °F | |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Mold Temperature | 32.0 °C | 89.6 °F | |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Mold Temperature | 32.0 - 60.0 °C | 89.6 - 140 °F | |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |
|||
Mold Temperature | 32.0 - 60.0 °C | 89.6 - 140 °F | |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po.. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L.. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® 351 High Performance Flame Retardant Polystyrene
(discontinued **) High Vicat and heat reflection temperature, Custom colorsApplications: Injection molding, Gas-assist injection molding, Structural foam, TV cabinets, Electronic enclosuresThis is an impact grade of .. |
|||
Mold Temperature | 32.0 - 54.0 °C | 89.6 - 129 °F | |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |