Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 66.0 - 88.0 °C | 151 - 190 °F | |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |