Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 149 - 232 °C | 300 - 450 °F | Average value: 204 °C Grade Count:5 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Mold Temperature | 177 - 232 °C | 350 - 450 °F | Average value: 200 °C Grade Count:6 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |