Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 149 - 220 °C | 300 - 428 °F | Average value: 181 °C Grade Count:7 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Mold Temperature | 200 - 220 °C | 392 - 428 °F | |
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer
(discontinued **) Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature applica.. |
|||
Mold Temperature | 190 - 220 °C | 374 - 428 °F | |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Mold Temperature | 200 - 220 °C | 392 - 428 °F | |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Mold Temperature | 200 - 220 °C | 392 - 428 °F | |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Mold Temperature | 200 - 220 °C | 392 - 428 °F | |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Mold Temperature | 200 - 220 °C | 392 - 428 °F | |
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in .. |
|||
Mold Temperature | 200 - 220 °C | 392 - 428 °F | |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |
|||
Mold Temperature | 200 - 220 °C | 392 - 428 °F | |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |
|||
Mold Temperature | 200 - 220 °C | 392 - 428 °F | |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |