Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 32.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® F7080 Developmental Flame Retardant Polystyrene  (discontinued **)
Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® F7080UV Developmental Flame Retardant Polystyrene  (discontinued **)
Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® F7120 Developmental Flame Retardant Polystyrene  (discontinued **)
Features: High flow for thin wall partsGood balance of physical propertiesUL94 V-0 @ 1.5 mm for black color Good aesthetics for injection molding Applications:Large television cabinetsConsumer elect..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® 7001 High Performance Flame Retardant Polystyrene  (discontinued **)
Super high flow, Reduced processing temperatures, Reduced processing time, Improved aesthetics, Custom colorsApplications: Injection molding, Gas-assist injection molding, Hard to fill cavities, suc..
Mold Temperature 32.0 °C
89.6 °F
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 22% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 32.0 °C
89.6 °F
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 22% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer
Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® 7000 Flame Retardant Polystyrene
Features:General purpose workhorse resinGood flow for injection moldingUL94 V-0 @ 1.5 mm for all colors UL94 5VA rating FOAMED @ 4.6 mm, 0.87-1.07 g/cc density, natural colorCustom colors availableA..
Mold Temperature 32.0 - 60.0 °C
89.6 - 140 °F
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer
Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce..
Mold Temperature 32.0 - 60.0 °C
89.6 - 140 °F
Styrolution NAS® 90 High Performance Styrenic
NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla..
Mold Temperature 32.0 - 79.4 °C
89.6 - 175 °F
Average value: 52.6 °C Grade Count:47
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
Mold Temperature 32.0 °C
89.6 °F
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 32.0 °C
89.6 °F
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 22% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 32.0 - 60.0 °C
89.6 - 140 °F
Styrolution NAS® 21 Acrylic Copolymer
Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma..
Mold Temperature 32.0 - 60.0 °C
89.6 - 140 °F
Styrolution NAS® 30 Series High Performance Styrenic
It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene  (discontinued **)
Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene  (discontinued **)
Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene  (discontinued **)
Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® 351 High Performance Flame Retardant Polystyrene  (discontinued **)
High Vicat and heat reflection temperature, Custom colorsApplications: Injection molding, Gas-assist injection molding, Structural foam, TV cabinets, Electronic enclosuresThis is an impact grade of ..
Mold Temperature 32.0 - 54.0 °C
89.6 - 129 °F
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene  (discontinued **)
Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo..
Copyright © lookpolymers.com All Rights Reserved