Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 85.0 - 105 °C | 185 - 221 °F | |
NatureWorks® Ingeo™ 3801X Injection Grade PLA Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork.. |
|||
Mold Temperature | 85.0 - 105 °C | 185 - 221 °F | DAM |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
Mold Temperature | 85.0 - 105 °C | 185 - 221 °F | DAM |
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |
|||
Mold Temperature | 85.0 - 105 °C | 185 - 221 °F | DAM |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
Mold Temperature | 85.0 - 135 °C | 185 - 275 °F | DAM |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
Mold Temperature | 85.0 - 105 °C | 185 - 221 °F | DAM |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also.. |
|||
Mold Temperature | 85.0 °C | 185 °F | |
Tipco Tipcofil® AG 200 - 10% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 10% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Mold Temperature | 85.0 °C | 185 °F | |
Tipco Tipcofil® AGM 602 - 10% Mineral & 20% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 10% Mineral + 20% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Mold Temperature | 85.0 °C | 185 °F | |
Tipco Tipcofil® AM 300 - 15% Mineral Reinforced Nylon-6 Compound, with High Heat Stability 15% Mineral Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Mold Temperature | 85.0 - 120 °C | 185 - 248 °F | |
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Mold Temperature | 85.0 - 135 °C | 185 - 275 °F | DAM |
DuPont Performance Polymers Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA) Zytel® HTN54G35EF NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin, developed for electrical and electronics applications. It is also a PPA r.. |
|||
Mold Temperature | 85.0 - 105 °C | 185 - 221 °F | DAM |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
Mold Temperature | 85.0 - 130 °C | 185 - 266 °F | DAM |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret.. |
|||
Mold Temperature | 85.0 - 105 °C | 185 - 221 °F | DAM |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |