Polymer Property : Mold Temperature = 149 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 45.0 - 65.0 °C
113 - 149 °F
Injection Molding
Ineos ABS Lustran® 266 ABS, Transparent Grade
Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing...
Mold Temperature 45.0 - 65.0 °C
113 - 149 °F
Injection Molding
Ineos ABS Lustran® 288 ABS, Injection Molding Grade
Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati..
Mold Temperature 45.0 - 65.0 °C
113 - 149 °F
Injection Molding
Ineos ABS Lustran® 308 ABS, Medical Grade
Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi..
Mold Temperature 45.0 - 65.0 °C
113 - 149 °F
Injection Molding
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade
Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi..
Mold Temperature 55.0 - 65.0 °C
131 - 149 °F
(A/B)
Metabolix Mirelâ„¢ F1005 Injection Molding Grade PHA Bioplastic
Mirel F1005 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such..
Mold Temperature 55.0 - 65.0 °C
131 - 149 °F
(A/B)
Metabolix Mirelâ„¢ F1006 Injection Molding Grade PHA Bioplastic
Mirel F1006 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such..
Mold Temperature 55.0 - 65.0 °C
131 - 149 °F
(A/B)
Metabolix Mirelâ„¢ P1003 Injection Molding Grade PHA Bioplastic
Mirelâ„¢ P1003 is a general purpose injection molding material with high modulus.Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and ..
Mold Temperature 55.0 - 65.0 °C
131 - 149 °F
(A/B)
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic
Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba..
Mold Temperature 40.0 - 65.0 °C
104 - 149 °F
ISBM Injection Mold
Eastman Tritan TX1800 Copolyester
Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo..
Mold Temperature 40.0 - 65.0 °C
104 - 149 °F
ISBM Injection Mold
Eastman Tritan TX1801 Copolyester, Natural
Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo..
Mold Temperature 40.0 - 65.0 °C
104 - 149 °F
ISBM Injection Mold Temp.
Eastman Tritan WX500 Copolyester
Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati..
Mold Temperature 40.0 - 65.0 °C
104 - 149 °F
ISBM Injection Mold Temp.
Eastman Tritan WX510 Copolyester
Eastman Tritan WX510 is a transparent blue resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. ..