Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 95.0 - 125 °C | 203 - 257 °F | |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Mold Temperature | 95.0 - 125 °C | 203 - 257 °F | |
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high .. |
|||
Mold Temperature | 120 - 125 °C | 248 - 257 °F | |
BecauseWeCare BF90 Biodegradable Plastic Biodegradable and compostable product produced from corn and developed to break down within weeks in a compost environment, without leaving any harmful residues in the process. Certified to the vari.. |