Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 343 - 400 °C | 649 - 752 °F | Average value: 370 °C Grade Count:4 |
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7033 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY/EM Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8084/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8085/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8087/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8088/RD Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8089/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8124 Polyether imide, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7223 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7743 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8133 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8154/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8232 Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8374 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7742 Polyether imide, with glass fiber, demolding aid Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |