Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 335 °C | 617 - 635 °F | |
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Nozzle Temperature | 325 - 335 °C | 617 - 635 °F | |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Nozzle Temperature | 325 - 335 °C | 617 - 635 °F | |
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |