Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 315 °C | 599 °F | Injection Molding |
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |
|||
Nozzle Temperature | 315 - 335 °C | 599 - 635 °F | NH Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |