Polymer Property : Nozzle Temperature = 489 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 216 - 254 °C
421 - 489 °F
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav..
Nozzle Temperature 216 - 254 °C
421 - 489 °F
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over..
Nozzle Temperature 249 - 254 °C
480 - 489 °F
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
Nozzle Temperature 249 - 254 °C
480 - 489 °F
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
Nozzle Temperature 249 - 254 °C
480 - 489 °F
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..