Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 216 - 254 °C | 421 - 489 °F | |
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav.. |
|||
Nozzle Temperature | 216 - 232 °C | 421 - 450 °F | |
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE) Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p.. |
|||
Nozzle Temperature | 216 - 232 °C | 421 - 450 °F | |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |
|||
Nozzle Temperature | 216 - 254 °C | 421 - 489 °F | |
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over.. |
|||
Nozzle Temperature | 216 °C | 421 °F | Injection |
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane Features: Low Compression SetUse: Hydraulic Seals and Gaskets Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Nozzle Temperature | 216 °C | 421 °F | Injection |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |