Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | Average value: 330 °C Grade Count:28 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | Average value: 330 °C Grade Count:22 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | Average value: 330 °C Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7329/GY PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7662/BK PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically .. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7836 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts.High dim.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Nozzle Temperature | 330 - 340 °C | 626 - 644 °F | |
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Nozzle Temperature | 330 - 340 °C | 626 - 644 °F | |
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Nozzle Temperature | 330 - 340 °C | 626 - 644 °F | |
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Nozzle Temperature | 330 - 340 °C | 626 - 644 °F | |
Lehmann & Voss LUVOCOM® 21-8015 Polyamide 6/6T, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8144 PPS, linear, with mineral filler Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low waterabsorbtion.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |
|||
Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |